AASHTO PP 100-20 for ultrathin bonded wearing course includes a mix design evaluation for the asphalt surface mixture, usually 1/2 to 1 in. (12.5 to 25.4 mm) thick, to determine the proportions of polymer-modified emulsified asphalt that is used as the tack coat, PG binder, mineral aggregate, mineral filler, and additives to produce an ultrathin bonded wearing course job-mix formula.
Product Details
Published: 2020 Number of Pages: 5 File Size: 1 file , 900 KB Product Code(s): PP100-20-UL, PP100-20-UL, PP100-20-UL